Document Type : Research Paper
Authors
Department of Chemistry, North Tehran Branch, Islamic Azad University, Tehran, Iran
Abstract
The recovery of selenium from Iranian sar-cheshmeh copper anode slime has been investigated. Copper anode slimes are containing varying precious metals, such as: gold, silver, selenium and tellurium. They are being extracted as a by-product in the production process. Arsenic and antimony that present in anode slimes dissolved in 0.4 M KOH. Then, the alkaline roasting of anode slimes in the presence of Na2CO3 solubilized selenium. Various parameters such as time and temperature of alkaline roasting were studied. The results indicated that the optimum condition for the temperature and time of roasting found to be T=600C and time= 8 h respectively, and that optimum recovery of selenium was 98%.